Abstract

A process for producing a biaxially-oriented multilayer film, comprising: (a) extruding a tubular multilayer tape comprising: (i) a first outer layer comprising a polyolefin, (ii) a second, core layer comprising a polyamide blend comprising nylon 6 blended with at least about 5% by weight of copolyamide, (iii) a third layer which is a core layer comprising polyolefin or an oxygen-barrier layer comprising at least one member selected from ethylene/vinyl alcohol copolymer, polyvinylidene chloride copolymer and polyacrylonitrile, and (iv) a fourth, outer layer comprising a polyolefin; (b) inflating the tape so that the tape is biaxially oriented by stretching in a transverse direction and machine direction, so that a tubular multilayer film is formed.

Term

Term ended

Projected expiry passed 4 June 2013, 13.3 years ago.

  1. Priority
  2. Filed
  3. Published
  4. Projected expiry
  5. Today

14 claims: 6 independent, 8 dependent

  1. 1
    A process for producing a biaxially-oriented multilayer film, comprising:(a) extruding a tubular multilayer tape comprising: (i) a first, outer layer comprising a polyolefin,(ii) a second, core layer comprising a polyamide blend comprising nylon 6 blended with at least about 5% by weight of copolyamide,(iii) a third layer which is a core layer comprising polyolefin or an oxygen-barrier layer comprising at least one member selected from ethylene/vinyl alcohol copolymer, polyvinylidene chloride copolymer and polyacrylonitrile, and(iv) a fourth, outer layer comprising a polyolefin;(b) inflating the tape so that the tape is biaxially oriented by stretching in a transverse direction and machine direction, so that a tubular multilayer film is formed.
  2. 6
    A process according to any one of the preceding claims, wherein the second polyamide layer comprises less than 15% of the total thickness of the structure.
  3. 7
    A process according to any one of the preceding claims, wherein the tape further comprises a fifth tie layer between the first outer polyolefin layer and second polyamide layer and a sixth tie layer between (a) the second polyamide layer and third core layer comprising polyolefin or (b) third oxygen-barrier layer and the fourth outer polyolefin layer.
  4. 9
    A process according to any one of the preceding claims, wherein:the first outer polyolefin layer comprises 20% by weight ethylene alpha-olefin copolymer and 80% by weight ethylene vinyl acetate copolymer;the third layer is a core polyolefin layer comprising 20% by weight ethylene alpha olefin copolymer and 80% by weight ethylene vinyl acetate copolymer, andthe fourth outer polyolefin layer comprises 80% by weight ethylene alpha-olefin copolymer and 20% by weight ionomer.
  5. 11
    A process according to any one of the preceding claims, wherein biaxial orientation is carried out at an orientation temperature of from 71 to 138°C (160 to 280°F).
  6. 14
    A process according to any one of the preceding claims, further comprising the step of coating an outside surface of the tubular multilayer film with oil.