PL425253A1

Method for producing carbon nanolayers on surfaces at the time of micro-smoothing them with abrasive films

Abstract

A method of producing carbon nanowayers with a thickness of 10-50 nanometers produced in the process of micro-smoothing the surface using diamond abrasive films (2) with grain sizes of 0.5 - 3 µm.

Term

No projected expiry on record.

  1. Priority and filed
  2. Published
  3. Today