Nova Patents
EP2016972A2

Lubricious coatings

Abstract

The present disclosure provides substrates having a lubricious coating thereon. The substrate may be flexible and include, in embodiments, a medical device. The lubricious coating, in embodiments, is applied in a pattern so that the coating avoids delamination and/or fracturing which might otherwise occur as the substrate flexes and/or stretches. The pattern comprises a dot matrix. For example the coating may be applied to a cannula seal, the cannula itself, and/or an instrument passing therethrough.

EP2016972A2, drawing sheet 1
Sheet 1 of 6

Term

Projected expiry 14 July 2028.

  1. Priority
  2. Filed
  3. Published
  4. Today
  5. Projected expiry

14 claims: 9 independent, 5 dependent

  1. 1
    An article comprising:a substrate;and a patterned lubricious coating comprising a dot matrix pattern on at least a portion of said substrate.
  2. 3
    A method comprising:providing a substrate;applying to the substrate a lubricious coating in a dot matrix pattern.
  3. 6
    The method of any one of claims 3 to 5 or the article of any one of claims 1, 2 or 5, wherein the lubricious coating is selected from the group consisting of cyanoacrylates, epoxies, hydrophilic polymers, hydrogels, polyalkylene oxides, urethanes, polyurethanes, siloxanes, cyclosiloxanes, polyalkylsiloxanes, polydialkylsiloxanes, parylenes, and combinations thereof.
  4. 7
    The method of any one of claims 3 to 6 or the article of any one of claims 1, 2 or 6, wherein the lubricious coating is selected from the group consisting of polyethylene oxide, polypropylene oxide, polyethylene oxide/polypropylene oxide copolymers, polyethylene glycol, polypropylene glycol, polydimethylsiloxanes, polydiethylsiloxanes, polydipropylsiloxanes, polydibutylsiloxanes, parylene N, parylene C, parylene D, parylene HT, and combinations thereof.
  5. 8
    The method of any one of claims 3 to 7, wherein the lubricious coating is applied by a method selected from the group consisting of gravure coating, spray coating, melt blowing, flexographic printing, screen printing, and combinations thereof.
  6. 9
    The method of any one of claims 3 to 8, wherein the lubricious coating is applied in powder form.
  7. 10
    The method of any one of claims 3 to 8, wherein the lubricious coating is applied as a coating solution including a solvent selected from the group consisting of tetrahydrofuran, methylene chloride, methanol, ethanol, propanol, chloroform, 1,2-dichloro-ethane, hexane, heptene, ethyl acetate, and combinations thereof.
  8. 12
    The method of any one of claims 3 to 11, further comprising heating the lubricious coating to a temperature from about 80°F to about 350°F.
  9. 13
    The method of any one of claims 3 to 12 or the article of any one of claims 1, 2 or 5 to 7, wherein the substrate possesses a coating-free surface area of from about 75% to about 99%.