Nova Patents
EP1908520A1

Peroxide-degrading catalyst

Abstract

An object of the present invention is to provide a catalyst which decomposes a peroxide effectively and economically under a high temperature while suppressing generation of free radicals, and the present invention provides a peroxide decomposition catalyst containing a base metal atom, wherein a value A indicating a free radical generation amount represented by the (equation 1) is not more than 0.20, and a value B indicating a reaction rate represented by the (equation 2), which can be easily applied to utility such as an agent for preventing deterioration of a polymer electrolyte-type fuel cell and a water electrolysis apparatus, and an antioxidant for medicaments, agrochemicals and foods. A=MwS/Mw-1 (wherein Mw is a weight average molecular weight of poly (sodium 4-styrenesulfonate) after a hydrogen peroxide decomposition test in the test at 80°C in the presence of poly(sodium 4-styrenesulfonate), and Mw(S) is a weight average molecular weight of poly(sodium 4-styrenesulfonate) before the test) B=NPO/Ncat (wherein N (po) is a mole number of hydrogen peroxide decomposed per 20 minutes in a hydrogen peroxide decomposition test in the (equation 1), and N(cat) is a mole number per metal atom of a catalyst used)

EP1908520A1, drawing sheet 1
Sheet 1 of 36

Term

Term ended

Projected expiry passed 20 June 2026, 0.3 years ago.

  1. Priority
  2. Filed
  3. Published
  4. Projected expiry
  5. Today

13 claims: 2 independent, 11 dependent

  1. 1
    A peroxide decomposition catalyst comprising abase metal atom, wherein a value A indicating a free radical generation amount represented by the (equation 1) is not more than 0.20, and a value B indicating a reaction rate represented by the (equation 2) is not less than 60. A = ( Mw ( S ) / Mw ) - 1 (wherein Mw is a weight average molecular weight of poly (sodium 4-styrenesulfonate) after a hydrogen peroxide decomposition test in the test at 80°C in the presence of poly(sodium 4-styrenesulfonate), and Mw is (S) is a weight average molecular weight of poly(sodium 4-styrenesulfonate) before the test) B = N ( po ) / N ( cat ) (wherein N (po) is a mole number of hydrogen peroxide decomposed per 20 minutes in the hydrogen peroxide decomposition test in the (equation 1), and N (cat) is a mole number of a catalyst used per metal atom)
  2. 9
    The peroxide decomposition catalyst according to any one of claims 1 to 8, wherein the catalyst decomposes hydrogen peroxide.
  3. 10
    A method of decomposing a peroxide, comprising decomposing a peroxide at not lower than 45°C using the peroxide decomposition catalyst according to any one of claims 1 to 8.
  4. 11
    A method of analyzing a radical, comprising quantitating a radical by a change in a molecular weight of an aliphatic polymer using the aliphatic polymer as a radical detecting agent.