EP0882003B1

Alkylation of benzene to form linear alkylbenzenes using fluorin e-containing mordenites

Abstract

This record has no abstract on file.

EP0882003B1, drawing sheet 1
Sheet 1 of 3

Term

Term ended

Expired 10 February 2017, 9.6 years ago.

  1. Priority
  2. Filed
  3. Granted
  4. Expired
  5. Today

12 claims: 12 independent, 0 dependent

  1. 1
    A process useful for the production of monoalkylated benzene, comprising:contacting benzene with an olefin of from 8 to 30 carbons in the presence of fluorine-containing mordenite under conditions such that monoalkylated benzene is formed;wherein the mordenite has been treated by contacting mordenite with an aqueous hydrogen fluoride solution, wherein the hydrogen fluoride in the aqueous solution has a concentration in the range from 0.1 to 1 percent by weight, wherein the contacting occurs at a temperature of from 0°C to 50°C for a time sufficient to provide a fluorine content in the mordenite of from 0.1 to 4 percent by weight. Procédé utile pour la production de benzène monoalkylé, comprenant l'étape consistant : à mettre en contact du benzène avec une oléfine ayant de 8 à 30 atomes de carbone en présence d'une mordénite conte-nant du fluor dans des conditions telles que du benzène monoalkylé est formé ;dans lequel la mordénite a été traitée en mettant en contact la mordénite avec une solution de fluorure d'hydrogène aqueuse, dans lequel le fluorure d'hydrogène dans la solution aqueuse possède une concentration dans la gamme de 0,1 à 1 pour cent en poids,    dans lequel la mise en contact se produit à une température allant de 0°C à 50°C pendant une durée suffisante pour fournir une teneur en fluor, allant de 0,1 à 4 pour cent en poids, dans la mordénite. Verfahren, das zur Herstellung von monoalkyliertem Benzol nützlich ist, welches umfaßt: Inkontaktbringen von Benzol mit einem Olefin mit von 8 bis 30 Kohlenstoffen in Gegenwart von Fluor enthaltendem Mordenit unter solchen Bedingungen, daß monoalkyliertes Benzol gebildet wird;wobei das Mordenit durch Inkontaktbringen von Mordenit mit einer wäßrigen Fluorwasserstofflösung behandelt worden ist, wobei der Fluorwasserstoff in der wäßrigen Lösung eine Konzentration im Bereich von 0,1 bis 1 Gewichtsprozent besitzt, wobei das Inkontaktbringen bei einer Temperatur von 0°C bis 50°C für einen Zeitraum eintritt, der ausreichend ist, um im Mordenit einen Fluor-Gehalt von 0,1 bis 4 Gewichtsprozent bereitzustellen.
  2. 2
    Procédé selon la revendication 1, dans lequel la mordénite contenant du fluor possède un rapport molaire silice à alumine dans une gamme de 10:1 à 50:1. The process of claim 1, wherein the fluorine-containing mordenite has a silica to alumina molar ratio in a range from 10:1 to 50:1. Verfahren nach Anspruch 1, dadurch gekennzeichnet, daß das Fluor enthaltende Mordenit ein Siliziumdioxid-zu-Aluminiumoxid-Molverhältnis in einem Bereich von 10:1 bis 50:1 besitzt.
  3. 3
    Procédé selon la revendication 1 ou 2, dans lequel l'oléfine possède de 10 à 14 atomes de carbone. The process of claim 1 or 2, wherein the olefin has from 10 to 14 carbons. Verfahren nach Anspruch 1 oder 2, dadurch gekennzeichnet, daß das Olefin von 10 bis 14 Kohlenstoffe besitzt.
  4. 4
    Procédé selon l'une quelconque des revendications précédentes, comprenant de plus l'étape consistant :à laisser le benzène, l'oléfine et le benzène monoalkylé descendre dans un rebouilleur à partir du lit de catalyseur ;à éliminer le benzène monoalkylé du rebouilleur ;età chauffer le contenu du rebouilleur de façon telle que le benzène reflue pour être en contact supplémentaire avec la mordénite contenant du fluor. The process of any of the preceding claims further comprising: allowing benzene, olefin, and monoalkylated benzene to descend into a reboiler from the catalyst bed;removing monoalkylated benzene from the reboiler;andheating the contents of the reboiler such that benzene refluxes to further contact the fluorine-containing mordenite. Verfahren nach einem der vorangehenden Ansprüche, dadurch gekennzeichnet, daß es weiter umfaßt: Absteigenlassen von Benzol, Olefin und monoalkyliertem Benzol aus dem Katalysatorbett in einen Reboiler;Entfernen von monoalkyliertem Benzol aus dem Reboiler;undErhitzen des Inhaltes des Reboilers, so daß Benzol unter Rückfluß kocht, um weiter in Kontakt mit dem Fluor enthaltenden Mordenit zu kommen.
  5. 5
    Procédé selon la revendication 4, dans lequel le rapport benzène à oléfine dans l'alimentation est de 2:1 à 20:1, dans lequel le lit de catalyseur est maintenu à une température de 75°C à 200°C, et dans lequel l'alimentation est introduite dans le lit de catalyseur à une vitesse spatiale horaire de liquide de 0,1 h-1 à 1 h-1. The process of claim 4, wherein the benzene to olefin ratio in the feed is 2:1 to 20:1, wherein the catalyst bed is maintained at a temperature of 75°C to 200°C, and wherein the feed is introduced into the catalyst bed at a liquid hourly space velocity of 0.1 hr-1 to 1 hr-1. Verfahren nach Anspruch 4, dadurch gekennzeichnet, daß das Verhältnis von Benzol zu Olefin in der Beschickung 2:1 bis 20:1 beträgt, daß das Katalysatorbett bei einer Temperatur von 75°C bis 200°C gehalten wird und daß die Beschickung in das Katalysatorbett mit einer stündlichen Flüssigkeitsraumgeschwindigkeit von 0,1 h-1 bis 1 h-1 eingebracht wird.
  6. 6
    Procédé selon l'une quelconque des revendications 1 à 3, dans lequel le rapport benzène à oléfine est de 2:1 à 20:1, dans lequel la mordénite contenant du fluor est maintenue à une température dans une gamme de 75°C à 200°C, et dans lequel le benzène et l'oléfine sont introduits dans la mordénite contenant du fluor à une vitesse spatiale horaire de liquide de 0,1 h-1 à 1 h-1. The process of any of claims claims 1 to 3, wherein the benzene to olefin ratio is 2:1 to 20:1, wherein the fluorine-containing mordenite is maintained at a temperature in a range from 75°C to 200°C, and wherein the benzene and olefin is introduced into the fluorine-containing mordenite at a liquid hourly space velocity of 0.1 hr-1 to 1 hr-1. Verfahren nach einem der Ansprüche 1 bis 3, dadurch gekennzeichnet, daß das Verhältnis von Benzol zu Olefin 2:1 bis 20:1 beträgt, daß das Fluor enthaltende Mordenit bei einer Temperatur im Bereich von 75°C bis 200°C gehalten wird und daß das Benzol und das Olefin in das Fluor enthaltende Mordenit mit einer stündlichen Flüssigkeitsraumgeschwindigkeit von 0,1 h-1 bis 1 h-1 eingebracht werden.
  7. 7
    Process according to any of the preceding claims, wherein a temperature in the range from 80°C to 140°C is maintained during the contacting step of benzene and the olefin. Procédé selon l'une quelconque des revendications précédentes, dans lequel une température dans la gamme de 80°C à 140°C est maintenue au cours de l'étape de mise en contact du benzène et de l'oléfine. Verfahren nach einem der vorangehenden Ansprüche, dadurch gekennzeichnet, daß eine Temperatur im Bereich von 80°C bis 140°C während des Kontaktschrittes von Benzol und dem Olefin aufrechterhalten wird.
  8. 8
    Procédé selon la revendication 4 ou 5, comprenant de plus étape consistant à recueillir l'eau en tête du lit de catalyseur dans un piège à eau. The process of claim 4 or 5 further comprising collecting water overhead to the catalyst bed in a water trap. Verfahren nach Anspruch 4 oder 5, dadurch gekennzeichnet, daß es weiterhin das Sammeln von Wasser oberhalb des Kopfes des Katalysatorbettes in einer Wasserfalle umfaßt.
  9. 9
    Mordenit, das nützlich ist zur Alkylierung von Benzol mit Olefin, mit einem Siliziumdioxid-zu-Aluminiumoxid-Molverhältnis in einem Bereich von 10:1 bis 100:1;wobei das Mordenit mit einer wäßrigen Fluorwasserstofflösung mit einer Konzentration im Bereich von 0,1 bis 1 Gewichtsprozent behandelt worden ist, wobei das Inkontaktbringen bei einer Temperatur von 0°C bis 50°C für einen Zeitraum eintritt, der ausreichend ist, um einen Fluor-Gehalt im Mordenit von 0,1 bis 4 Gewichtsprozent bereitzustellen. Mordenite useful for alkylating benzene with olefin having a silica to alumina molar ratio in a range from 10:1 to 100:1;wherein the mordenite has been treated with an aqueous hydrogen fluoride solution having a concentration in the range from 0.1 to 1 percent by weight, wherein the contacting occurs at a temperature of from 0°C to 50°C for a time sufficient to provide a fluorine content in the mordenite of from 0.1 to 4 percent by weight. Mordénite utile pour alkyler du benzène avec une oléfine possédant un rapport molaire silice à alumine dans une gamme de 10:1 à 100:1 ;dans lequel la mordénite a été traitée avec une solution de fluorure d'hydrogène aqueuse possédant une concentration dans la gamme de 0,1 à 1 pour cent en poids,    dans lequel la mise en contact se produit à une température allant de 0°C à 50°C pendant une durée suffisante pour fournir une teneur en fluor, allant de 0,1 à 4 pour cent en poids, dans la mordénite.
  10. 10
    Mordenit nach Anspruch 9, dadurch gekennzeichnet, daß das Siliziumdioxid-zu-Aluminiumoxid-Molverhältnis 10:1 bis 50:1 beträgt. Mordénite selon la revendication 9, dans laquelle le rapport molaire silice à alumine est de 10:1 à 50:1. The mordenite of claim 9, wherein the silica to alumina molar ratio is 10:1 to 50:1.
  11. 11
    A method useful for the preparation of fluorine-containing mordenite, comprising:contacting a mordenite having a silica to alumina molar ratio in a range from 10:1 to 100:1 with an aqueous hydrogen fluoride solution having a concentration in the range from 0.1 to 1 percent by weight, wherein the contacting occurs at a temperature of from 0°C to 50°C for a time sufficient to provide a fluorine content in the mordenite of from 0.1 to 4 percent by weight;collecting the fluorine-containing mordenite by filtration;anddrying the collected fluorine-containing mordenite. Procédé utile pour la préparation de mordénite contenant du fluor, comprenant l'étape consistant : à mettre en contact une mordénite possédant un rapport molaire silice à alumine dans une gamme de 10:1 à 100:1 avec une solution de fluorure d'hydrogène aqueuse possédant une concentration dans la gamme de 0,1 à 1 pour cent en poids, dans lequel la mise en contact se produit à une température allant de 0°C à 50°C pendant une durée suffisante pour fournir une teneur en fluor, allant de 0,1 à 4 pour cent en poids, dans la mordénite ;à recueillir par filtration la mordénite contenant du fluor ;età sécher la mordénite contenant du fluor. Verfahren, das zur Herstellung von Fluor enthaltendem Mordenit nützlich ist, welches umfaßt: Inkontaktbringen eines Mordenits mit einem Siliziumdioxid-zu-Aluminiumoxid-Molverhältnis in einem Bereich von 10:1 bis 100:1 mit einer wäßrigen Fluorwasserstofflösung mit einer Konzentration im Bereich von 0,1 bis 1 Gewichtsprozent, wobei das Inkontaktbringen bei einer Temperatur von 0°C bis 50°C für einen Zeitraum eintritt, der ausreichend ist, um einen Fluor-Gehalt im Mordenit von 0,1 bis 4 Gewichtsprozent bereitzustellen;Sammeln des Fluor enthaltenden Mordenits durch Filtration;undTrocknen des gesammelten, Fluor enthaltenden Mordenits.
  12. 12
    Procédé selon la revendication 11, dans lequel le rapport molaire silice à alumine est de 50:1 ou inférieur. The method of claim 11, wherein the silica to alumina molar ratio is 50:1 or less. Verfahren nach Anspruch 11, dadurch gekennzeichnet, daß das Siliziumdioxid-zu-Aluminiuoxid-Molverhältnis 50:1 oder weniger beträgt.