EP0678488A2

Process for preparing solidified material containing coal ash.

Abstract

A process for preparing a solidified material containing a coal ash comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, a second step of molding the mixture to obtain a molded article, and a third step of subjecting the molded article obtained in the second step to a hydrothermal treatment at a temperature of 120°C or more under a high pressure. In the first step, 40 to 95 parts by weight of the coal ash is mixed with 60 to 5 parts by weight of the calcium compound, and the coal ash to be used has a bulk density of 0.8 g/cm³ or more, an average particle diameter of 5 to 40 µm and an aluminum content of 35% by weight or less in terms of Al₂O₃. By the use of a blowing agent or the like, it is also possible to obtain a porous light-weight solid. In consequence, there can be obtained the solid containing the coal ash and having a high mixing ratio of the coal ash, an excellent dimensional stability to water, a high strength and a decreased unevenness of the strength, and this kind of solid can be applied to many fields as building materials, construction materials, artificial aggregates and the like. Furthermore, a laminated solid having not only the above-mentioned characteristics but also weight reduction properties can also be obtained, and this solid can be suitably applied to building materials such as panels, blocks, bricks and boards for accoustic use, artificial light-weight aggregates and the like. Accordingly, the coal ash which is an industrial waste can be effectively utilized in large quantities, so that the conventional hard and troublesome problem of treating the coal ash can be solved or relieved.

EP0678488A2, drawing sheet 1
Sheet 1 of 7

Term

Term ended

Projected expiry passed 13 March 2015, 11.5 years ago.

  1. Priority
  2. Filed
  3. Published
  4. Projected expiry
  5. Today

7 claims: 6 independent, 1 dependent

  1. 1
    A process for preparing a solidified material containing a coal ash which comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, and a second step of molding the mixture to obtain a molded article,    the coal ash having a bulk density of 0.8 g/cm³ or more and an average particle diameter of 5 to 40 µm,    an aluminum content in the coal ash being 35% by weight or less in terms of Al₂O₃,    in the first step, 40 to 95 parts by weight of the coal ash being mixed with 60 to 5 parts by weight of the calcium compound, and    after the second step, a third step being carried out in which the molded article obtained in the second step is subjected to a hydrothermal treatment at a temperature of 120°C or more under a high pressure.
  2. 2
    A process for preparing a solidified material containing a coal ash which comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, and a second step of molding the mixture to obtain a molded article,    the coal ash having a bulk density of 0.8 g/cm³ or more and an average particle diameter of 5 to 40 µm,    an aluminum content in the coal ash being 35% by weight or less in terms of Al₂O₃,    in the first step, 40 to 90 parts by weight of the coal ash being mixed with 60 to 10 parts by weight of the calcium compound, one selected from the group consisting of a blowing agent and a foaming agent, and water, and    after the second step, a third step being carried out in which the molded article obtained in the second step is subjected to a hydrothermal treatment at a temperature of 120°C or more under a high pressure.
  3. 3
    A process for preparing a solidified material containing a coal ash which comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, and a second step of molding the mixture to obtain a molded article,    the coal ash having a bulk density of 0.8 g/cm³ or more and an average particle diameter of 5 to 40 µm,    an aluminum content in the coal ash being 35% by weight or less in terms of Al₂O₃,    in the first step, 40 to 90 parts by weight of the coal ash being mixed with 60 to 10 parts by weight of the calcium compound and water, and air bubbles being blown imto this mixture, and    after the second step, a third step being carried out in which the molded article obtained in the second step is subjected to a hydrothermal treatment at a temperature of 120°C or more under a high pressure.
  4. 4
    A process for preparing a solidified material containing a coal ash which comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, and a second step of molding the mixture to obtain a molded article,    the coal ash having a bulk density of 0.8 g/cm³ or more and an average particle diameter of 5 to 40 µm,    an aluminum content in the coal ash being 35% by weight or less in terms of Al₂O₃,    in the first step, 10 to 90 parts by weight of the coal ash being mixed with 90 to 10 parts by weight of the calcium compound, one selected from the group consisting of a blowing agent and a foaming agent, and water to obtain two or more mixtures which are different from each other in at least one selected from the group consisting of the kinds and amounts of coal ash, calcium compound, blowing agent or foaming agent, and water,    in the second step, the two or more mixtures being molded in a laminate state, and    after the second step, a third step being carried out in which the molded article obtained in the second step is subjected to a hydrothermal treatment at a temperature of 120°C or more under a high pressure.
  5. 5
    A process for preparing a solidified material containing a coal ash which comprises a first step of mixing the coal ash with a calcium compound to obtain a mixture, and a second step of molding the mixture to obtain a molded article,    the coal ash having a bulk density of 0.8 g/cm³ or more and an average particle diameter of 5 to 40 µm,    an aluminum content in the coal ash being 35% by weight or less in terms of Al₂O₃,    in the first step, 10 to 90 parts by weight of the coal ash being mixed with 90 to 10 parts by weight of the calcium compound and water to obtain two or more mixtures which are different from each other in at least one selected from the group consisting of the kinds and amounts of coal ash, calcium compound and water, and a predetermined amount of air bubbles is blown into each of the two or more mixtures,    in the second step, the two or more mixtures being molded in a laminate state, and    after the second step, a third step being carried out in which the molded article obtained in the second step is subjected to a hydrothermal treatment at a temperature of 120°C or more under a high pressure.
  6. 6
    The process for preparing a solidified material containing a coal ash according to any one of Claims 1 to 5 wherein the molded article obtained in the second step is cured at 30 to 100°C, prior to the third step.
  7. 7
    The process for preparing a solidified material containing a coal ash according to Claims 1 to 5 wherein the calcium compound is one or any combination of calcium compounds selected from the group consisting of calcium oxide, calcium hydroxide, calcium carbonate and calcium silicate.