AT359310T

Polyurethane elastomers having improved physical properties and a process for the production thereof

Abstract

A number average molecular weight of 1,000 to 3,000 Daltons polyol composition, comprising: (1) At least 60% weights' the compound content is parts of propylene polyol, a molecular weight of 2000 to 12,000 Daltons, the non-degree saturation of less than or equal to the 0.02meq/g and (2) is not more than 40% wt% the molecular weight of about 400 to 1,000 Daltons polyatomic alcohol, wherein the disperse index is greater than 1.1. The method for polyol component has good the physical and mechanical property polyurethane elastomer with diisocyanate, the polyisocyanate and isocyanate terminated prepolymer body or prepolymer for preparation of isocyanate terminated. The method of any known preparing polyurethane elastomer, comprising a one-step method, used for the preparation of the invention claims.

Term

No projected expiry on record.

  1. Priority
  2. Filed
  3. Granted
  4. Today

23 members in 11 offices

This recordMember, by publication datePriority claim1 more office is in the list below

Priority claims1

Priority claims
DocumentOfficeKindDate
9423802United States of AmericaA

Members23

Family members, oldest first
DocumentOfficeKind
CA2420833A1CanadaA1
EP1342740A1European Patent Office (EPO)A1
US2003176615A1United States of AmericaA1
KR20030074157ARepublic of KoreaA
CN1443793AChinaA
JP2003286326AJapanA
MXPA03001992AMexicoA
US6824703B2United States of AmericaB2
US2005027096A1United States of AmericaA1
US7045650B2United States of AmericaB2
US2006149021A1United States of AmericaA1
EP1342740B1European Patent Office (EPO)B1
CN1310992CChinaC
AT359310TThis recordAustriaT
DE60313068D1GermanyD1
DK1342740T3DenmarkT3
ES2284992T3SpainT3
DE60313068T2GermanyT2
JP2008208386AJapanA
US7511111B2United States of AmericaB2
JP4272453B2JapanB2
CA2420833CCanadaC
JP2014088583AJapanA