AT305022T

Polyolefin materials having enhanced surface durability

Abstract

The shaped article according invention claims a thermoplastic polymer blend is made, wherein with high performance of such as high the bearing, buprenorphine and a resilient. Thermoplastic formed polyolefin and about 40%~ about 80% to the propylene polymer basic components; 5%~ Between about 30% and; And about 5%~ about 30% thermoplastic elastic preferably, the content of styrene block or random copolymer. Thermoplastic preferably formed polyolefin and about 50%~ about 70% basic components; 10%~ Between about 20% and; And about 5%~ about 20% styrene block copolymers. , Wherein the thermoplastic elastomer comprising a higher than wt% of styrene monomers advantageously.

Term

No projected expiry on record.

  1. Priority
  2. Filed
  3. Granted
  4. Today

17 members in 11 offices

This recordMember, by publication datePriority claim1 more office is in the list below

Priority claims2

Priority claims
DocumentOfficeKindDate
57566000United States of AmericaA
0117224United States of AmericaW

Members17

Family members, oldest first
DocumentOfficeKind
CA2410486A1CanadaA1
WO0192404A1World Intellectual Property Organization (WIPO)A1
AU6347501AAustraliaA
KR20030014676ARepublic of KoreaA
EP1294803A1European Patent Office (EPO)A1
MXPA02011711AMexicoA
US6541568B1United States of AmericaB1
CN1437636AChinaA
JP2003535176AJapanA
EP1294803A4European Patent Office (EPO)A4
EP1294803B1European Patent Office (EPO)B1
AT305022TThis recordAustriaT
ATE305022T1AustriaT1
DE60113534D1GermanyD1
DE60113534T2GermanyT2
KR100808036B1Republic of KoreaB1
CA2410486CCanadaC